RE: [MW:33900] Re: ASTM A53 Gr.B TYPE E equivalent in ASTM

EN 10217-1 does not contain S275JR. S275JR is a structural steel acc to EN 10025-2. It covers plates and open sections – not pipes.

Structural pipes is found in EN 10210 and EN 10219.

 

EN 10217-1 is for pipes for pressure purposes and have type P195, P235 and P265.

 

Kind regards

Kristian Lund Jepsen

Senior Chief Consultant

 

D +45 51617324

M +45 51617324

kuj@ramboll.com

Rambøll Danmark A/S, DK REG. NO. 35128417
Registered office: Hannemanns Allé 53, 2300 Copenhagen S

 

From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf Of Kannayeram Gnanapandithan
Sent: 5. januar 2023 10:48
To: materials-welding@googlegroups.com
Subject: Re: [MW:33895] Re: ASTM A53 Gr.B TYPE E equivalent in ASTM

 

ASTM A 53 is a Pipe material specification


THANKS & BEST REGARDS,

KG.PANDITHAN, BE, IWE,  CSWIP 3.1,

ISO 9712 Level 2 in VT,

ASNT-Level II in PT,MT,RT & UT,

LA ISO 9001-2015,

International Welding Engineer. 

CONSULTANT-WELDING & QUALITY

Mobile no: +919940739349

 

 

On Thu, Jan 5, 2023 at 12:04 PM Vishwas Keskar Welding Manager WELDING <vvkeskar123@gmail.com> wrote:

Pl. prepare comparative statement in detail  for both the Materials of interest.

Consult Engineer - Design

Jointly discuss the service application of the component under fabrication for which you are intending to change the MOC and then decide the material selection .

 

Regards

 

Vishwas -IWE 

International Welding Engineer

 

On Thursday, January 5, 2023 at 9:33:30 AM UTC+5:30 Sami MERT wrote:

Dear All,

 

Is ASTM A53 Gr.B TYPE E equivalent properties with S275JR (EN 10217-1) ? Could we use it instead of ASTM A53 Gr.B TYPE E?

 

Best Regards

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b9c7a47d-885a-4e6a-bbc4-6f11afa99ad7n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNmySJbxQGxaauDfHGoyc2xRqVnhC3-t9giD7dMVT%3Dwbg%40mail.gmail.com.


Classification: Confidential

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...