Re: [MW:33650] ER-70S-2 and ER70S-6

no restrictions  but pl verify the BTC for ER 70S-6 chemistry which Mn, Si shall be within A1 maximum limit. (Mn-1,6, Si-0,8)

On Tue, Nov 1, 2022, 2:47 PM Muhammad Azeem <azeem7999@gmail.com> wrote:

Hi Zafar,
As per approved WPS you need to follow the same filler wire or electrode, You can switch for welders within the same F number and can use any filler wire.
For WPS strict to utilized as per Actual PQR.

Regards,

Muhammad Azeem Iqbal
Welding Inspector Aramco Approved
053110-8577/0554453626/0590071467




On Mon, 31 Oct 2022 at 06:12, Chaudhary Zafar Iqbal <chzaiqbal88@gmail.com> wrote:
Respected Member of this Group ,

As per approved wps ER70S-2 required to use .


Any code restrictions to use ER70S-6 instead of ER-70S-2 ?

Any code restriction and reference to change the WPS ?

Waiting for your valuable comments .

Regards,
Zafar 
00966544639978

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP9k9Xfz8xCCsA_t9CeOMw_Z506BBi5sX5wjT8SUuBrS9JrsZQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHqH7yCo0g6%3DZQJ82zq0zhu9fPU%3DLsgQcu0AFDbFdUvoo08_dg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eP3CbwCre5ZZp0hrmooO1A%2BRaf6JD-1kn2hd2rw%3DxRiRg%40mail.gmail.com.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...