Skip to main content

Re: [MW:32823] Re: Selection of Pigs For 30" Gas Pipeline

Dear ASIF

It can be done by special pigging method. 
The pig will move with crawler. 
We have done for 20 km.
Just float the enquiry and pigging companies will quote you

Regards
Shabbir Ahmad

On Tue, Feb 8, 2022 at 6:20 AM Mohd Siraj <mohd52100@gmail.com> wrote:
dear,
refer attached PDF,

 I studied, your pdf loops, I think this is code boundary B31.3 for the above ground and valve section area, pigging is done for UG Pipeline. check if any code boundary piping.,

i prefer to divide your section into subsections and prefabricated Pig-launcher and Pig receiver.

you need to divide it into subsections and add golden joint (100% Rt/+100% Ut) after the hydro test. since pigging require or use during hydro testing.

as per the below mail reply from Mr. Goswami, you need professional support from the company or else if u have a competent team to do, u can do so.

for pigging selection.
1. form pig'
2. clean pig ( with the brush)
3. hydro test pigging (double side)
4. caliper pigging
5. gouging pigging.



On Monday, January 17, 2022 at 6:18:41 AM UTC+3 Engr. Asif Chowdhury wrote:
Dear Experts,

Hope everyone is doing great.

In a cross country gas pipeline project over a bridge deck we have almost completed ou welding activities and right now we are facing problem in selection of Pigs for that pipeline.
 
For your information, the pipeline is about approximately 6 Km in length consisting of  14 nos U-loop and 06 Nos W-loop and 01 nos inlet and 01 nos outlet loops. Outer Dia of Pipeline is about 762 mm with a wall thickness of 25.4 mm.

The elbows in the loops are 1.5D 90 Degree LR BW elbows.

The entire pipeline has some pipe miter joints included but the angle of miter falls between the range of 2.5 Degree to  5 Degree.

 The normal pigs we use for our cross country pipeline having 3D & 5D Bends are not suitable here.

As I have limited knowledge on pigging, hope some expert comment can help me to select the appropriate pig and finalize procurement for my project in Bangladesh.


With best regards,
Asif
PM
PMB-NGP Project
WhatsApp: +8801925-884133
The Royal Utilisation Services (Pvt.) Ltd.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9de1e91f-9dec-442e-9f1a-126d96c426e8n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAH9U03x%2BH%3D0YcrQw3i8dEu1DOZh%3DzjSSp0S6cCFXyZN-KrY02A%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Re: [MW:14950] RE: 14919] Stress relieving Rejected for 5 min less soaking time.

Dear All, I have been a CONSULTANT FOR such problem & my personal opinion is expressed as follow. I fully agree with views expressed so far. But bag to differ that " Code is a law, with engineering judgments. Hence the inspector has the rights to declare that the original HT was inadequate." Inspectors & total industry must resist the "REJECTION" . We as intellectual & having seniority must become practical. How the code will revise???. ANS.: One is experiments (Pure research) & second is such chances that gives opportunity to experiment !!! _______________________________________________________________________________________________ My understanding is that it is P1 material. In that case every pass normalizes the immediate bottom pass. Hence code requirement for P1 FOR MANDATORY SR is 32 mm & above thickness. SOLUTION:  In any case 0. After SR=PWHT no PTC testing is required as per code--Unless for low temp. vessels. That means code ...