Skip to main content

[MW:32896] FW: 32891] RE: 32887] Qualification of WPS for DSS

 

Hi,

 

Your query does not specify the intended service? However, application of Duplex Stainless steels in pipelines are typically for offshore O&G carrying and processing pipelines. DNV guidelines are followed a lot for such design conditions. You may take a look at this attached specification and read through some of the highlighted guidelines. Usually for such pipelines involving Duplex Stainless Steels many of the technical requirements are client driven. If your project has specific requirements those would be more binding that the attached specification.

 

 

Thanks.

 

 

Pradip Goswami.P.Eng, IWE.

Independent Welding & Metallurgical Engineering Specialist)

Saudi Aramco Approved Designated Project Welding Engineer (DPWR)

Qatar Petroleum Approved, SME-Materials & Corrosion Engineering.

Email:pgoswami@rogers.com,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

 

From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf of Benaouda Mezrar

Sent: February 17, 2022 5:15 AM

To: Materials & Welding <materials-welding@googlegroups.com>

Subject: [MW:32887] Qualification of WPS for DSS

 

 

Hi expert

 

In which code I can find the essential variable for qualification of the WPS for DSS pipeline thanks for your help friend and have good day

 

 

--

https://materials-welding.blogspot.com/

https://www.linkedin.com/groups/122787

---

You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com <mailto:materials-welding+unsubscribe@googlegroups.com> .

To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1a4d5a1a-9635-42b4-a2d5-acb0b900097dn%40googlegroups.com <https://groups.google.com/d/msgid/materials-welding/1a4d5a1a-9635-42b4-a2d5-acb0b900097dn%40googlegroups.com?utm_medium=email&utm_source=footer> .

 

 

 

________________________________

 

<https://www.avg.com/internet-security>   This email has been checked for viruses by AVG antivirus software.

www.avg.com <https://www.avg.com/internet-security> 

 

 

 

 

--

https://materials-welding.blogspot.com/

https://www.linkedin.com/groups/122787

---

You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com <mailto:materials-welding+unsubscribe@googlegroups.com> .

To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAuAAAAAAAAABVPzeizzeRJsiPziIE5jXQBAMO2jhD3dRHOtM0AqgC7tuYAAAAAAA4AABAAAADWLpon/diTQqsz0R8H27cbAQAAAAA%3D%40rogers.com <https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAuAAAAAAAAABVPzeizzeRJsiPziIE5jXQBAMO2jhD3dRHOtM0AqgC7tuYAAAAAAA4AABAAAADWLpon/diTQqsz0R8H27cbAQAAAAA%3D%40rogers.com?utm_medium=email&utm_source=footer> .

 




AVG logo

This email has been checked for viruses by AVG antivirus software.
www.avg.com


Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Re: [MW:14950] RE: 14919] Stress relieving Rejected for 5 min less soaking time.

Dear All, I have been a CONSULTANT FOR such problem & my personal opinion is expressed as follow. I fully agree with views expressed so far. But bag to differ that " Code is a law, with engineering judgments. Hence the inspector has the rights to declare that the original HT was inadequate." Inspectors & total industry must resist the "REJECTION" . We as intellectual & having seniority must become practical. How the code will revise???. ANS.: One is experiments (Pure research) & second is such chances that gives opportunity to experiment !!! _______________________________________________________________________________________________ My understanding is that it is P1 material. In that case every pass normalizes the immediate bottom pass. Hence code requirement for P1 FOR MANDATORY SR is 32 mm & above thickness. SOLUTION:  In any case 0. After SR=PWHT no PTC testing is required as per code--Unless for low temp. vessels. That means code ...