[MW:32805] Re: QW 200.4: Combination of Welding Procedures

"Question: While combining the two PQRs to weld a plate with the thickness(es) ranging from 1.5 mm to 16 mm."

pl, check one is semiautomatic and one is a manual process, I don't see benefits of the combination.?...

furthermore,
welding Root wirh SMAW and over it SAW OR welding Root with SAW over it SMAW does make welding complex.



On Wednesday, December 29, 2021 at 6:35:29 AM UTC+3 Sudhakar Kuppuswamy wrote:

Hi,


Currently one of my clients is having an ambiguity in applying the requirements of ASME Section 09 Clause QW 200.4: Combination of Welding Procedures, Subclause:  a & b requirements. Hence, support is required in finding an interpretation from ASME Section 09. (Interpretation in CS connect is not apparent for this clause)

Background: Two PQRs were qualified separately, PQR A is qualified with SAW process using 8 mm thickness plate and PQR B is qualified with SMAW process using 8 mm thickness plate.

Question: While combining the two PQRs to weld a plate with thickness(es) ranging from 1.5 mm to 16 mm.

Do as per QW 200.4, it is necessary to have the root pass process PQR need to be qualified on a minimum 13 mm thickness plate?

I'm pretty sure it is not required to have a root pass process PQR with minimum 13 mm thickness in the above case. However, it would be helpful if you found any interpretation on this.


Regards,

Sudhakar K CEng MWeldI,IWE.

Welding & Metallurgical Engineer,

Email: sudhak...@gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5773e14a-e4c7-4c2c-8138-cf9ea43dcc05n%40googlegroups.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Re: [MW:14950] RE: 14919] Stress relieving Rejected for 5 min less soaking time.

Dear All, I have been a CONSULTANT FOR such problem & my personal opinion is expressed as follow. I fully agree with views expressed so far. But bag to differ that " Code is a law, with engineering judgments. Hence the inspector has the rights to declare that the original HT was inadequate." Inspectors & total industry must resist the "REJECTION" . We as intellectual & having seniority must become practical. How the code will revise???. ANS.: One is experiments (Pure research) & second is such chances that gives opportunity to experiment !!! _______________________________________________________________________________________________ My understanding is that it is P1 material. In that case every pass normalizes the immediate bottom pass. Hence code requirement for P1 FOR MANDATORY SR is 32 mm & above thickness. SOLUTION:  In any case 0. After SR=PWHT no PTC testing is required as per code--Unless for low temp. vessels. That means code ...