Re: [MW:32323] PMI for ASTM A105 Flanges

I suppose this issue may be due to non-availability of MTC or due to Heat Number Traceability. If this is the case, then PMI by suitable methods to reveal the chemical composition of the Flange an option

Thanks & Regards

J.Gerald Jayakumar




On Thursday, 22 April, 2021, 09:12:44 am IST, Babur Khan <mbabur.bwp@gmail.com> wrote:


Dear Experts,
One of our contractor purposed PMI for ASTM A105 Flanges due to lake of inspection documents.
As my understanding PMI is suitable for HSLAS,
SS and DSS. For carbon Steel we can check if there is something happened im change of welding consumables for welding.
Please share your experience.

Babur Khan Lashari

Sent from my iPhone

Muhammad Babur Khan
Sent from my iPhone

--
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/F2094BAB-A558-456E-9910-FD7962768B98%40gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...