Friday, April 16, 2021

Re: [MW:32267] Hydrotesting Calculation of Steel pipeline

Dear Sir,

The Operating pressure is 19 bar & the Max Allowable Pressure is 32 Bar &with Operating Temp is 32-degree Celcius. 

I need the Standard Deadweight testing calculations formula with the Procedure which is used in CGD.







On Wed, Apr 14, 2021 at 8:26 PM Vinay Thattey <vinay.thattey@gmail.com> wrote:
Dear Tejas ;

it's a schedule 20 pipeline . But you need to know about design pressure OR maximum allowable operating pressure  and also operating temp
erature 
Generally, (gas )pipelines are hydrotested by filling the test section of pipe with water and pumping the pressure up to a value that is higher than maximum allowable operating pressure (MAOP) and holding the pressure for a period of four to eight hours.

On Wed, 14 Apr 2021 at 10:15, tejas kerzare <tejas.kerzare3@gmail.com> wrote:
Dear All,

Please can you Provide Hydrotesting calculation of the steel pipeline having pipe API 5L Grade B.
Pipe Size - 10 Inch 
Thickness -  6.4 mm
Total Length of Steel pipeline - 1000M.

Thanking You!

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPv03FtvoiimrgkJqacUt3MM-e8yQ4W-tPc7r%3D_3oAYFMb3mhw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BQ29Oib1u-UMfyoZ4tYH%3D8dLLxQME3bTsBq5vPNBzw%2BaKvq9g%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPv03FufbMs2F770y9tdL90%3D3esgFz82HrTYjMyDvZn%2BMjhFOg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...