Re: [MW:32256] welding api 5l x52 with x60

i mean the anchor flange astm a694 f60

Le jeu. 15 avr. 2021 à 08:38, QA/QC <adnanziad49@gmail.com> a écrit :
Dear master 
i have a approved wps for welding api 5l x52  pipeline and i want to weld a anchor flange x60 is the wps cover it or we should requlaify it again 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c82adcc6-aec4-4acc-9815-966de7fd1a23n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACbfGKdx6_oS8JYenXW8gx83EDru5v1ope1aGuaTVsxQZ04%3Dtw%40mail.gmail.com.

No comments:

[MW:35742] PQR- Chemical testing requirements