Dear Experts,
One of our contractor purposed PMI for ASTM A105 Flanges due to lake of inspection documents.
As my understanding PMI is suitable for HSLAS,
SS and DSS. For carbon Steel we can check if there is something happened im change of welding consumables for welding.
Please share your experience.
Babur Khan Lashari
Sent from my iPhone
Muhammad Babur Khan
Sent from my iPhone
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/F2094BAB-A558-456E-9910-FD7962768B98%40gmail.com.
Subscribe to:
Post Comments (Atom)
[MW:35692]
Dear all Can I do MPI above painting surface for cs tank Regards, Sriram Srinivasan -- https://materials-welding.blog...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment