QW 402 - Joint design - GTAW - Backing - With/Without
(Ref - QW256- GTAW - QW 402.5- Addition of backing is Non essential variable.)
if Both (Backing - With/Without ) is addressed( which like normally is addressed), then there is no issue at all .
Eg-
QW 402-
Backing: With/Without
Root spacing: As per piping fabrication drawing
Backing Material (Type): Yes (Metal)
1. Metal - 2. Non-fusing Metal
3. Nonmetallic NA 4. OthersThe matter is to be resolved amicably . Meet QAC In charge along with Welding Engineer, Manufacturing Responsible. Explain him the details .
It shall be acceptable.
Regards
On Monday, April 19, 2021 at 7:20:46 AM UTC+4 sankar krishnan wrote:
Dear Gentlemen,Good Evening, In our project Vessel joint thickness 10mm ,Process(GTAW+SAW),Single V jointThey completed Welding ,Few days later during Inspection we observed , They have done Internal Welding of the shell, As per WPS its not shownGuys let me Know its can Accepted or RejectedIf Rejected , Please send Reference code standardsAs per QW 402.5 Joints (Backing its non Essential ),Its mention Backing strip or also back welding
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/960d2caa-6684-4216-b79d-6eb48095898cn%40googlegroups.com.
Comments