Sunday, April 18, 2021

[MW:32276] Welding consumables for the CS with Inconel 625 clad pipe joints weld

Dear all,

 

Please give me the welding consumables for the CS with Inconel 625 clad pipe joints weld.

 

For Inconel 625 we can use ER NiCrMo-3 and E NiCrMo-3. If we use this electrode then the cost will be more.

 

Is there any alternative electrode (Like 7018 )we can use for filling and capping of CS in this CS with inconel 625 clad pipe joints?


Thank you.

pkm

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFoQ_newcdaMwr%3Dr8ECJ9W5_MOjVMB2MLb3KkpV_WKNKD2PU8w%40mail.gmail.com.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...