Skip to main content

Re: [MW:31939] WPS-Lost test Reports

Dear Jamie,

WPS/PQR/WPQ was qualified in accordance with AWS D1.1

Yes the testing was done at an accredited third party lab and we have the test certificates from the lab stating that the PQR was used to qualify the welders.

On Mon, Jan 18, 2021 at 4:36 PM Jamie Reyes <jamiejrmachineco@gmail.com> wrote:
What was the code that was used to qualify the WPS/PQR/WPQ?

Were the PQR/WPQ test specimens tested at an accredited third-party lab? If so, do you still have the test certifications from the third-party lab stating acceptance, with the PQR that was used and other info etc. noted on the test certification(s)? 







On Sun, Jan 17, 2021 at 7:05 PM 'Anumiah Veera Jegan' via Materials & Welding <materials-welding@googlegroups.com> wrote:

Dear all,

We currently have a WPS with us.But due to some documentation error the PQR was lost.Is the WPS still valid(we've been using it for years).Does this also make the welders qualified based on this WPS invalid?.Thanks

The information contained in this e-mail may be privileged and confidential. If the reader is not the intended recipient, or agent of the intended recipient, any unauthorised use, disclosure, copying, distribution or dissemination is strictly prohibited. If you have received this communication in error, please notify the sender immediately and delete it from your system.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d5e7f7ec-afee-4dc8-8581-58a09910c26cn%40googlegroups.com.
--
Regards,
Jamie Reyes
J.R. Machine Company, Inc.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJNUtUP75NgtpZXZetbdvkv_Vqgt4wK%2B1eqdMdafGV3vTrc3uw%40mail.gmail.com.


--
Displaying
Regards,
Anumiah Veera Jegan
Certified Welding Inspector
Ley Choon Group
No 3 Sungei Kadut Drive Singapore 729556
Office Tel: (65) 6757-0900 | Fax: (65) 6757-0100
Website: www.leychoon.com

The information contained in this e-mail may be privileged and confidential. If the reader is not the intended recipient, or agent of the intended recipient, any unauthorised use, disclosure, copying, distribution or dissemination is strictly prohibited. If you have received this communication in error, please notify the sender immediately and delete it from your system.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEQjo%2BS5QNutDm02CetgGh_78V%2BnJ9UwH7SDi27MFho%3DaV6Mmg%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...