Dear Asif
       you may use below electrodes for given materials.

1- GTAW  - ER80S-B2
2- SMAW  - E8018G


Regards
Dinesh Kumar Gaur

On Monday, 4 January, 2021, 09:17:15 am IST, Engr. Asif Chowdhury <al.istiaque09@gmail.com> wrote:


Dear All Concern,

Please help me selection for welding of pipe materials as per following spec:

Pipe Spec: 

1. NB: 750 mm; WT: 25.4 mm; API 5L -X65M, PSL -2, LSAW, ASTM B36.10M

2. NB: 200 mm; SCH: XS; API 5L -X65M, PSL -2, SMLS, ASTM B36.10M

3. NB: 100 mm; SCH: XS; API 5L -X65M, PSL -2, SMLS, ASTM B36.10M

Minimum Yield Strength of Pipe : 450 MPa

Ultimate Tensile Strength of Pipe : 535 MPa

My client wants me to do GTAW for Root & Hot passes and SMAW for Filling & Capping Passes. 

I wish for everyone's sound health and sound mind. 

Thanks In Advance,

Md. Asif Al-Istiaque Chowdhury
Manager (Project Sales & Operation)
WhatsApp No.: +88 01925-884133

The Royal Utilisation Services (Pvt.) Ltd.
(An ISO 9001:2008 Certified Company)
House # 383 (3rd Floor), Road # 28,
New DOHS, Mohakhali, Dhaka-1206, Bangladesh.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/efaf3bef-3826-4097-bf55-d092c6c0850an%40googlegroups.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...