Re: [MW:31881] Tubes expansion beyond drum thickness.

What is  expansion % ?


On Fri, Dec 25, 2020 at 3:57 PM Neeraj Yadav <neeru25oct@gmail.com> wrote:
Dear experts,

We are executing a project for 35 TPH Natural Gas fired Auxiliary Boiler designed for max. working pressure of 60 kg/cm2 and steam temperature of 392 Deg .Cel.

All water tubes of boiler are connected to steam( 63 mm Thk) & Mud drum(40mm Thk) with expanded design of construction.

In mud drum it is observed that tubes ( 51X4 mm) are expanded upto 30mm more than the drum thickness and indicating as bulged. we have checked the OD at bulged part and observed 1-2 mm flared and thickness around 3.5 mm

Kindly advise weather it is acceptable or we have to replace the se tubes with reference to code. Code of construction is ASME Sec-1/IBR.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bbc02a3f-f869-4c58-a898-ed522ce25df6n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3NhrooefyO9THOePDw%2BKV2E%2B5raJ1R4u%2B7epndeCvhhDw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...