Friday, December 18, 2020

Re: [MW:31871] Subject:- Charpy Impact Testing on weld metal

Hello Pradip sir,
Sir, can you say about, any metallurgical difference we get on the fracture surface and is there any change in fractography on both v and u notch test samples  

On Fri, Dec 18, 2020 at 10:37 AM <pgoswami@rogers.com> wrote:

U- Notch for Charpy impact tests used to be followed  DIN standards, back in 1970s. In fact DIN standards used to provide an option for both Notch types. Correlation of impact data was never easy.   It's discarded since then.

It's a matter of basic understanding : a V notch generates more stress than an U-Notch, Hence materials exhibiting good impact with V Notched specimens  would easily meet the criteria in U-Notch conditions not the other way. Notch toughness is an extremely critical property for engineering design.

Anything good under worse condition(V-Notch) is more reliable that something performed under ideal condition (U-Notch). Engineering codes, material properties  have matured  and improved leaps and bounds over the. Hence adoption of V-Notch Charpy impact test is an example of that principle.

Hope it clears your doubts.

Thanks.

 

Pradip Goswami.P.Eng, IWE.

Independent  & Consulting Welding & Metallurgical Specialist

Saudi Aramco Approved Designated Welding Engineer(DPWR)

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@rogers.com,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf Of Shahil Saini
Sent: December 17, 2020 3:49 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:31868] Subject:- Charpy Impact Testing on weld metal

 

That I know sir, but I want some more information behind this topic why they discarded U notch and For every material they are not using U notch or for which materials U notch is used?

 

On Thu 17 Dec, 2020, 9:17 AM George Dilintas, <dilintas@gmail.com> wrote:

V notch simulation is more reliable 

 

Στις Τετ, 16 Δεκ 2020, 06:58 ο χρήστης Shahil Saini <sainishahil98@gmail.com> έγραψε:

Hello everyone, 

 

My question is, Why ASME BPVC and other standard codes discarded the 'U' notch impact testing?

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALfBO_9KBo5H3LU6KOD1xU1LpWHVZwm5SJq4-Z%3DkQDprJTQTrw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40DBBBfmR6sVKsFeL2w_g8SD3Hb1Tv3fu79ZK6TNi_1%3DCA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALfBO__W5fmuqoj4BVvrg4%3DgUJfmFvtUVhG_JHNr5Av14QAAxg%40mail.gmail.com.


Virus-free. www.avg.com

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAuAAAAAAAAABVPzeizzeRJsiPziIE5jXQBAMO2jhD3dRHOtM0AqgC7tuYAAAAAAA4AABAAAACMo9pg8L3gT5rx4MIIKFOuAQAAAAA%3D%40rogers.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALfBO_8pk-Z1-UWdabk6usDdjGKjXUYtYdHMsXBL-RjVKp0Ucg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...