if code of construction is ASME sec1, it is required or if it is Sec8, preheat is enough upto 38mm
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE, CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer.
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349
On Thu, Dec 17, 2020 at 10:33 AM furkan topaloğlu <topaloglufurkan8@gmail.com> wrote:
In order to reduce the risk of cold cracks due to thickness and stress, PWHT can be applied to provide slow cooling after welding.Jamie Reyes <jamiejrmachineco@gmail.com>, 17 Ara 2020 Per, 06:55 tarihinde şunu yazdı:What is the code of construction?What is the type of service?Is Lethal Services involved?Need the above mentioned information.....Regards,Jamie ReyesJ.R. Machine Company, Inc.--On Wed, Dec 16, 2020 at 7:47 PM thanh tung Nguyen <tungexp.268@gmail.com> wrote:Dear Experts,--Hope you all are well.I have a question is about the weld of the base material of CS (or Low temp. CS) with wall thickness greater than 25mm, Do we still required PWHT if we applied a preheating process before, or PWHT is no longer mandatory?And which reference can be found?Thank you & best regards./.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKr%2BxwbEWDaz5Lo9eQpu_iY7m4Gewk3V9A%3D556vTj9QwUkBHQQ%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJNUtUPCr_fxg1Ep1iYS-ozi5XG1vBHajiJ_Sf06paBaW9R97g%40mail.gmail.com.
----Regards / Saygılarımla
Furkan TOPALOĞLU
Metallurgy and Material & Welding Engineer
Metalurji ve Malzeme & Kaynak Mühendisi
Phone : +90 (539) 437 88 03
E-Mail : topaloglufurkan8@gmail.com
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALZR%3D4SC_A6X9qw-8Xvf5Gpw6YVgy1MnN9QpVBegJLNurqrxuQ%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNje5ucSzaH7YsKrdW%3DObdZUdF1HfgrLULbuNcNOAj%2Bpg%40mail.gmail.com.
Comments