Re: [MW:31857] PWHT Requirement for Supports?

Pwht is governed by the pressure part, not by the support. If the support is welded on a pressure part which must be pwhted then this weld will be pwhted

Στις Τετ, 16 Δεκ 2020, 08:34 ο χρήστης bilal wahla <bilalwahla047@gmail.com> έγραψε:

Greeting ALL,

On my project we are doing PWHT on Thickness basis, Pipe thickness is 30.18mm
,Will we do PWHT of Welded Supports as per B31.3? 


Bilal Arshad 
P.W.H.T QCI 

Mobile: +966 580181061

Email: bilalwahla.047@gmail.com

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMqL%2BROYYc4qzhMs9p%3Dr39KsXvUZXYe32G-CAYZ%2BBW3sj-K1wA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40C5Dr3mBaSn0oi%3D0rA0Sc0qjr8jfYcfjg9YA60_YuZGWA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...