Hi,

Please refer to NACE TM0284, for the measurement of cracks with respect to crack sensitivity ratio (CSR), crack length ratio (CLR), and crack thickness ratio (CTR).,



R Albert Anbarasan 




On Monday, December 14, 2020, 12:07:26 PM GMT+8, asghar...@gmail.com <asgharialigl@gmail.com> wrote:


Dear All.
Does any body have any experience about measuring of the gap between edges of crack especially for HIC or SWC? and which method would be useful?
Regards, 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f7fbe2f6-94d9-41a3-9cf9-558a6d579c14n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...