Thursday, December 10, 2020

Re: [MW:31829] Instrument recommendation for stellite welding deposition check after final machining

Coating thickness gauge / coat metre may be used, provided weld deposition is on magnetic material.

Prasad G

On Thu, 10 Dec 2020, 14:58 SURESH, <qms.pjgpl@gmail.com> wrote:
Dear Experts
Need suggestion on how to check deposition of stellite welding ERCoCr-B on Duplex stainless steel.

Customer requirement is minimum 0.8mm deposition of hard-faced welding on the base material. We have made 1.6mm welded and final machined as per drawing dimension. My query is how to check the deposition of weld on the base material. Is there any instrument or method is there to check. Kindly suggest

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f7bbe4cf-b3cc-474b-a057-604aedde46ebn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEi5r3YwOrcEQUVnPdT6WmrbDL8Q2ipCXo_nvSamaOp%3DHf1whw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...