Thursday, December 3, 2020

Re: [MW:31806] PWHT REQUIRED OR NOT?

Mr.Patel, Doesn't require any PWHT after explosive cladding.  
if the customer wants you can, otherwise not.


On Thu, Dec 3, 2020 at 8:34 AM Patel Ankit <aapatel271@gmail.com> wrote:
Yes sir,

After Bonding PWHT required or not??

On Thu 3 Dec, 2020, 9:00 AM George Dilintas, <dilintas@gmail.com> wrote:
What do you mean by bonding

Στις Τετ, 2 Δεκ 2020 στις 5:12 π.μ., ο/η Patel Ankit <aapatel271@gmail.com> έγραψε:
Dear Expert,

I hope all are well.

My question is In after Tubesheet Bonding PWHT required or Not?

Base Material : SA 516 GR 70. (Thk : 45 mm )
Bonding Material : SA 240 GR 316. (Thk:5mm)

Tubesheet Dia : 3000 mm

( Note : Bonding plate SS 316 : 1 No joint on base material)

Regards,
Ankit Patel
8140255303.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALR-PuwRp0-NoHz6KXB6-4Y3tkTKmaB4pJxtF8HhM8ctpf3EtA%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40CjGONDt6HonTPf4vP1h_MmXkyu76RSLh7pykTRw10Uig%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALR-PuyDQdbY3rMmc%2BFcZVTP%2BvFyX4r5MJt5Lnkhjw7kbA7x_Q%40mail.gmail.com.


--
With Regards

Udaya bahaskar.D

+919676270121

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANii3RNRi9qNctSjHmBcOy07SeeJd%3DohSRNQMoOqWUPb0bSAuA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...