Hello everyone, 

My question is, Why ASME BPVC and other standard codes discarded the 'U' notch impact testing?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALfBO_9KBo5H3LU6KOD1xU1LpWHVZwm5SJq4-Z%3DkQDprJTQTrw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS