Dear Giants,
-- I want to know about little doubt on piping welding repair WPS.
WPS made with 6010 and 7010 electrodes for regular welding.
Now I can plan with 6010 and 7018 electrodes for Repair WPS on the same .
Material :API5L PSL2 grade P1G1
is it allowable?
please correct me.
-- With Regards
Udaya bahaskar.D