Dear Sandeep.
Thank you for sharing the link, but the only paragraph which talk about my concern is ''If the composite is a pipe or if it must be welded from one side, the buttering technique should be used. In this case the filler metal must provide an analysis equal to the clad metal and be compatible with the backing steel. Weld passes are made on the edge of the composite to butter the clad and backing metal. The buttering pass must be smoothed to the design dimensions prior to fitup. The same electrode can be used to make the join'' and again you have to deposit carbon steel filler metal on a buttering pass which is an alloyed metal.
I think the statement is not applicable for cladad piping.
Regards.

On Mon, Nov 23, 2020 at 5:17 PM Sandeep Pr <prsandeep61@gmail.com> wrote:

On Mon, Nov 23, 2020 at 7:37 AM Ali Asghari <asgharialigl@gmail.com> wrote:
Dear George.
Thank you for responding, but my question isn't related to your response, actually this statement siad when you have two clad components which want to be welded to each other, first base metal shall be welded and joined ,after that cladded parts.
Now what would be possible for welding of cladded small piping?
Regards,   

On Thu, Nov 19, 2020 at 3:02 PM George Dilintas <dilintas@gmail.com> wrote:
 If you deposit a cladding of 316 or 304 on a carbon steel, you may get hot cracking due to low Ferrite number. Therefore you deposit a layer of 309 which mixed with the carbon steel does not give hot cracking

Στις Δευ, 16 ĪĪæĪµ 2020, 16:38 Īæ Ļ‡ĻĪ®ĻƒĻ„Ī·Ļ‚ asghar...@gmail.com <asgharialigl@gmail.com> έγραψε:
Dear All.
Would you say what is the reason of this statement" When welding clad materials from both sides, the C and CMn steel shall be completely welded prior to welding the cladding. C or CMn steel or low alloyed steel weld metal shall not be deposited onto a high alloy base material or weld metal.'' ?
How is it possible for cladded piping?
Regards,

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4d8f2d92-d9ee-4ec7-89ca-ebdddd25d516n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/cHRITpDcpLU/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40AuqmjYA5cN4ciu_swJ0i%3DHQ6TFJqPFQ5fOD7Z57XWUUw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALcH7WD8bbTqFWLiZ_H-0OxUU5H0QbNM7qKsp9ubBDqMLCf0Aw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/cHRITpDcpLU/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFBEtQowRdWOo9-Y_N5Uh-fNzcVu3PnChZZ1N7ivwnG-xODOpA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALcH7WCuHuunosi1PjpsjmwqiCUG7%3DwPXgs7ZPV-2%2BNpJDi6XA%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...