Re: [MW:31773] P-No. in ASME-IX code

It was for Cast iron. Now it is totally deleted

On Mon, Nov 23, 2020, 7:17 PM Sandeep Pr <prsandeep61@gmail.com> wrote:

Dear Eng. Hany Nabil,


Kindly submit your query using this link

 

https://cstools.asme.org/Interpretation/InterpretationForm.cfm




With Regards,

Sandeep.P.Raghavan


On Mon, Nov 23, 2020 at 7:37 AM Hany Nabil <eng.hanynabil20@gmail.com> wrote:
Dear Exports,

as per table QW/QB-422 in ASME-IX code, the P-No. 2 is not used 
Why ?


 Best Regards,

 Eng. Hany Nabil
 Senior Welding Engineer
 Petrofac
 Engineering and Production Service
 Egypt Mobile: 002-01225622022



This message, including any attachments, may contain confidential and privileged information for the sole use of the intended recipient(s). Review, use, distribution or disclosure by others is strictly prohibited. If you are not the intended recipient, or authorised to receive information on behalf of the recipient, please contact the sender by reply email, and delete all copies of this message. While we have taken reasonable precautions to ensure that this message and any attachments are free from viruses, we cannot guarantee that they are virus free and accept no liability for any damage caused by this message or any attachments. Messages sent or received through our networks may be monitored to ensure compliance with the law, regulation and/or our policies.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP1YJmTbMbEri-cye4ny7kVm63_BykGTZW%3D2X6L%2B_8fLoP6E5w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFBEtQotxasERP5F76yJOz48dzjH2sKEQndcz8UX9p6sTz5T3A%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePDgNTwdDL%3D-izo9W-s7tZJkucSYv%3Da51wJMmgJ%2BB2B6Q%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...