Re: [MW:31772] Suitable welding electrode for IS 2707 Gr 2_Q & T

Correction 
Dear Mohammed,

After welding, did you only carry out the Quenching heat treatment...?
What about the "Tempering" part...?

Ramin  Kondori
Sr. QA/QC & Welding Engineer
-----------------------------------------------------------
PG-Dip. in Welding Engineering (IWE  AT  0070)
BSc. in Civil Engineering (IUT)
BGAS Painting Inspector
ASNT Level I&II
                        
IIW-Logo-Colour-small


On Mon, Nov 23, 2020 at 5:17 PM Mohammed Asan K S <asan.mohammed@manisfoundry.com> wrote:
Dear Sirs,,

We required the welding electrode for subjected grade and procedure for welding on the castings.
Already the job was welded by E9018M and found low hardness after quenching the job. To reach the 50 HRC, what is welding electrode to be used?

Thank you

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/01cacbad-a154-4114-b8d0-82417a5ec7e9n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEagfUia%3DREgJ3cbPEu0sCeAGxR6vXvp%3D2%3DQtkeyupx9RHdKOQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...