Re: [MW:31748] Query on root gap

Built up is the best way

Στις Πέμ, 19 Νοε 2020, 07:26 ο χρήστης 'Anumiah Veera Jegan' via Materials & Welding <materials-welding@googlegroups.com> έγραψε:
Dear experts,

Our client has allowed a root gap of 20mm in between pipelines. But due to some constraints the root gap will be more than the allowed limit. Can I know how to fill the gap(build up or use of a filler metal) as per AWS

Thanks

The information contained in this e-mail may be privileged and confidential. If the reader is not the intended recipient, or agent of the intended recipient, any unauthorised use, disclosure, copying, distribution or dissemination is strictly prohibited. If you have received this communication in error, please notify the sender immediately and delete it from your system.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2fce4b96-4263-4a7d-9627-2c7cb2f91af4n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40Aneb_1VqhQOLK8jy4XzxqALSUKHehgPKdZJPd9Xj4xxw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...