Re: [MW:31724] 431 to 630

what is chemistry of 610

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Sat, Nov 7, 2020 at 9:13 AM Vishwas Keskar <vvkeskar123@gmail.com> wrote:
Pl. send MTC
What is  service application?
What is type of joint?


On Fri, Nov 6, 2020 at 7:33 AM Pravin Poornachandran <htcispravin@gmail.com> wrote:
Dear Expert, 

Good day to you.

I'm looking for suitable consumable to weld 431 to 610. 
I have been searching and studying for this combination but it's difficult to get accurate information. 

Can anyone help? 

Best regards,
Pravin 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADDyn7e3e3hgc9ei9NBS5b4zu%3DyhMw_rjiSTR3K5TA0QL36erg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3MK75cSwO1vjA7dM2jF2iNxRkGwTvzE5Qdap%2B%2BqrgZx6w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePMR9ToGqw_a5kLG1zGixpZn5jOaN4jt5uQ-sWd3sKdbA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...