F-no. 5 with backing also qualifies F-No.1 with backing along with F-No. 5 with backing as per QW-433

On Tue, Nov 3, 2020 at 3:55 PM George Dilintas <dilintas@gmail.com> wrote:
see QW-433 in Section IX
F-no. 5 with backing qualifies only F-No. 5 with backing
F-No. 5 without backing qualifies only F-No. 1 with backing and F-No. 5 with and without backing

Στις Δευ, 2 Νοε 2020 στις 11:00 π.μ., ο/η NIKHIL THOMAS JOY <nikhil.thomasjoy@gmail.com> έγραψε:

Dear experts,

Greetings of the day

I have a query related to the F Number in welding process.

IF I QUALIFY A WELDER WITH F No.6, He can weld all F.No-6.

But, if I Qualify with F No.5, can he weld F No.1 to 4.

Experts please reply as per code reference.

BEST REGARDS,
NIKHIL THOMAS JOY
IWI LIMITED 
ADNOC-WHRP
0544975526

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJxkuiVye%3DvWpXy28w6g%2Bvj77vUNNQHJGZp6dUUi%2Bb5aD1oyOw%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40DCQ-SjNKkROHvWRG8eiLvAJobiTfoqMRgopkRs1baUGQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOBi_eOvLFwR7npHrmKSicgRP-Y%3DwPJh-iDMarEvVS80MQ2W9A%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...