Re: [MW:31708] Filler wire for welding EN36C plate

Pl. send MTC and min required TS YS ELON 

What is the service application ?
what is the type of joint ?

On Tue, Nov 3, 2020 at 9:36 AM GALAXY INDUSTRIES PRASHANT PANCHAL <pipanchal@live.com> wrote:
Dear Experts,

Kindly suggest which Filler wire to be used for welding EN36C  material.

Kindly acknowledge the same.

With Best Regards,

Prashant Panchal

M/s. Galaxy Industries,
R-386, TTC Industrial Estate,
Rabale, Navi – Mumbai-400701.
Mob: +91-98200-82842

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CY4PR20MB1574BCF9DCDBEE37575B454AC3110%40CY4PR20MB1574.namprd20.prod.outlook.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3N-X%2BxzXvt6taGHfM8ny5ykeOGjQDR%3DLZnzVEsWnQwWiQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...