Tuesday, November 3, 2020

Re: [MW:31706] PFI-ES-7-Min-Spacing-for-Welding : weld olet

It does not, but what prevails is the Code of Construction 
In case of VIII-1 UG refer to UG-39 & UG-42

Στις Παρ, 16 Οκτ 2020 στις 6:29 π.μ., ο/η anhtrangnghieng <anhtrangnghieng@gmail.com> έγραψε:

Dear Experts, 
 Refer to PFI-ES-7-Min-Spacing-for-Welding: Could you please advise the reason why this standard does not mention for size less than 2.1/2". 

Thanks in advance.




--



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADOyxJheVd9w4hO7rspFW8bqkuQGyGs_m3RwCyuxcosfp9O_sA%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40Dxv-6TvfDLqMMKT4SJHC4C3sfuquYRoBqYEok3V%3DGtAw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...