Tuesday, November 3, 2020

Re: [MW:31689] Please check

Dear Rajeev ;
You need to have circumferential welds to join two shell parts . A shell is rolled from a plate with seam welds . 

On Thu, 22 Oct 2020 at 10:05, Rajeev Shukla <gkpshuklaji@gmail.com> wrote:
Sir

I need to under stand the meaning of this line , and which code I should refer for Compressor received welding.

Longitudinal seam in adjacent sections shall not be in same line.

On Saturday, 21 April 2018 at 11:57:35 UTC+5:30 joykol...@gmail.com wrote:
Dear Expert,

Please suggest Dia range.for WPS as per API 1104.

--



Best Regards,

Joydev Dalai
Dy. Manager - QA/QC
Kalpataru Power Transmission ltd.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c23d7c90-1f2b-4a58-ab4d-651cbde1c374n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BQ29OiC63ssUfxaB3dAga2Oug9mkQ%2B2qXfHPwv9C1zxo%3Doqnw%40mail.gmail.com.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...