Hi Sir,

Thank you for your valuable input. Indeed we have to discuss with Client and Licensor about this requirement. Normally we just do the SP-7 as specified in API 936 but we would need to install acid coating that would require a more clean surface so it would not peel-off. Thus we may need to clarify with the Refractory Supplier about the required acid coating and its required surface preparation before we talk to Client/Licensor. 

Anyways, do you know what "63" means in the "SP 6-63"?
On Thursday, November 26, 2020 at 11:51:16 PM UTC+8 pgos...@rogers.com wrote:

Hi,

I think there're some mix-ups in the specifications and interpretations. SSPC SP6 or other specifications are applicable for  surface preparation by blasting for application of paints.

For the refractories the criteria is a bit different. Following is the extract from  API -936, for surface preparation before applications of refractory.

You may read the standard, discuss and settle the issue with the client based on the API-936 guidelines.

Thanks.

 

 

P.Goswami.P.Eng, IWE.

Independent  & Consulting Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgos...@rogers.com,pradip....@gmail.com

Cell/Whasapp:1-905-9793232

 

From: RKD <raymondkenn...@gmail.com>
Sent: November 26, 2020 10:15 AM
To: Materials & Welding <material...@googlegroups.com>
Subject: SSPC SP 6 - 63

 

Hello everyone.

 

I encountered a requirement from a Licensor specification that internal surface should be prepared as per SSPC SP 6 - 63 prior to refractory application.

 

I know SSPC SP 6 means commercial blast but I have never encountered or saw a surface preparation requirement "SP 6 - 63".

 

Does anyone know what this means?

 

Thank you in advance.


Virus-free. www.avg.com

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/dd6f9852-14ad-4624-916f-9c4acf80a29dn%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...