Monday, November 30, 2020

[MW:31786] Re: Different of EFW/ERW pipe

Hi, I am no expert but have you checked the material certificate of this piping to confirm the process used?

On Thursday, November 26, 2020 at 12:17:23 PM UTC+8 faizul wrote:
    Dear Expert,

    I come across with 2" pipe line which having appearance like using auto-weld process.
    From my understanding, electric fusion weld should be no filler rod used. However, from the actual piping at site, the weldment seem to have weld cap and show obvious long-seam appearance.
    I am never across with small diam of pipe having
  • Question: How do we know if the welding is electric fusion process or not? I am never across with small diam of pipe having long-seam appearance from outside

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/cfc63f2e-f4c7-4a99-89a9-c70e8395ed83n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...