Thursday, November 12, 2020

[MW:31734] Re: Imapct toughness testing on weld joint of material SA 516 Gr70

I agreed with Customer Care
Addition, I found problem in the PQR with actual test specimens that the subsize and reduction temperature not complied with UCS-66. You also check it out at UG-84.

On Tuesday, November 10, 2020 at 7:00:42 PM UTC+7 Shahil wrote:
Hello everyone, 
Can anyone help me in finding out problems arising during impact toughness testing of the weld joint of the pressure vessel.

Thank you,

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1ad5e4df-0c79-4c0c-a88f-97248bf4aa9dn%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...