Saturday, June 27, 2020

Re: [MW:31050] How to check Argon Gas Purity?

Normally you can get the Test certificate from the gas supplier about the purity of the gas.

Its enough to confirm the purity for WPS requirements.

என்றும் அன்புடன்,
Thanks & Regards,
RAJAVARMAN
+971561895584

On Fri, Jun 26, 2020, 7:35 PM Vinayak <vinayaknaik57@gmail.com> wrote:
what is the instrument name to check purity.

On Saturday, April 5, 2014 at 4:41:41 PM UTC+5:30, Richard robes wrote:
Mr.Prabhu,

You can check with Argon gas meter / Analyzer for 99.9 % purity or as per WPS requirements. Hope it's clear.

Regards
Richard


On Fri, Apr 4, 2014 at 4:18 PM, Maulik Thakkar <mlkth...@gmail.com> wrote:

You want to check which impurity?

Normally moisture/dew point need to be checked as per AWS 5.32. It should be less then 10.5 ppm.

To check moisture, dew point analyzer is available.

Regards,
Maulik
L&T, Welding engg. & Metallurgy

On Apr 4, 2014 5:31 PM, "prabhu" <prabhuj...@gmail.com> wrote:
Dear All,
 
I my doing work on SS material 316L , ensurinig clean and dust free area and surface but enable to rnsure the Argon gas purity.
please guid me how to ensure the gas .
Or is there any divice to check the Argon gas impurities.

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to material...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to material...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2b2c6a22-9f2c-4984-957c-4b0cebb443a0o%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BHpzU7bqMTz3ZRs7_2uZc98yoAbwmzT%3DysS0LAf%2BqhNvY_WnA%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...