Saturday, June 27, 2020

Re: [MW:31050] How to check Argon Gas Purity?


Hello;

Argon gas for shielding and purging during welding of SS and other corrosion resistant alloys including titanium

can be checked for purity by Weld Purge Monitors This instrument indicates the purity in pp or %age as required.

Huntingdon Fusion Techniques - UK are the pioneers in this field.See the link below:


In India contact www.weldwell.com exclusive distributor

Ashok Rai

On Sat, Jun 27, 2020 at 12:21 PM 'Karthik' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Hi,

Please find below the link might be useful to you.

https://news.thomasnet.com/fullstory/gas-analyzers-measure-trace-impurities-in-argon-826546

(PA - GOW-MAC Instrument Company, a leading manufacturer of gas analyzers and compressed gas handling equipment, offers the process oriented Series AR710 and AR720 Gas Analyzers with High Frequency Argon Discharge Ionization Detector (HFADD). The analyzers are offered as turnkey systems designed and optimized specifically for the analysis of trace impurities (i.e., H2, N2, O2, CH4, CO and CO2) in argon down to the part-per-billion (ppb) range. Two configurations are available depending upon the impurities being measured. Sensitivities of < 15 ppb can be measured)

SHAW Meter also can be used.

Thanks& Regards,

 

(Karthik)

Karthikeyan.S

M: +66-892512282
E-mail : karthik6684@yahoo.com



On Saturday, June 27, 2020, 10:08:29 AM GMT+7, 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:


Argon purity certificate comes from the Argon gas manufacturer which will be cross checked with the Batch Number on the cyclinder.

During Welding we only measure oxygen content in ppm levels using oxygen analyser and mentioned in the WPS

Thanks & Regards

J.Gerald Jayakumar




On Friday, June 26, 2020, 10:35:34 PM GMT+7, Vinayak <vinayaknaik57@gmail.com> wrote:


what is the instrument name to check purity.

On Saturday, April 5, 2014 at 4:41:41 PM UTC+5:30, Richard robes wrote:
Mr.Prabhu,

You can check with Argon gas meter / Analyzer for 99.9 % purity or as per WPS requirements. Hope it's clear.

Regards
Richard


On Fri, Apr 4, 2014 at 4:18 PM, Maulik Thakkar <mlkth...@gmail.com> wrote:

You want to check which impurity?

Normally moisture/dew point need to be checked as per AWS 5.32. It should be less then 10.5 ppm.

To check moisture, dew point analyzer is available.

Regards,
Maulik
L&T, Welding engg. & Metallurgy

On Apr 4, 2014 5:31 PM, "prabhu" <prabhuj...@gmail.com> wrote:
Dear All,
 
I my doing work on SS material 316L , ensurinig clean and dust free area and surface but enable to rnsure the Argon gas purity.
please guid me how to ensure the gas .
Or is there any divice to check the Argon gas impurities.

--
To post to this group, send email to material...@ googlegroups.com
To unsubscribe from this group, send email to material...@ googlegroups.com
For more options, visit this group's bolg at http://materials-welding. blogspot.com/
http://www.linkedin.com/ groups/MaterialsWelding- 122787?home=&gid=122787&trk= anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@ googlegroups.com.
For more options, visit https://groups.google.com/d/ optout.

--
To post to this group, send email to material...@ googlegroups.com
To unsubscribe from this group, send email to material...@ googlegroups.com
For more options, visit this group's bolg at http://materials-welding. blogspot.com/
http://www.linkedin.com/ groups/MaterialsWelding- 122787?home=&gid=122787&trk= anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@ googlegroups.com.
For more options, visit https://groups.google.com/d/ optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2b2c6a22-9f2c-4984-957c-4b0cebb443a0o%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/313981205.3112451.1593218482005%40mail.yahoo.com
.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1095365990.3149645.1593228740179%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJkv1VrGLbzAHGjaxD1%3D4ACgSiCR0zXvfSvngj4Rv_64zXnUtQ%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...