Re: [MW:30668] RT film size required

There is no requirement for width. 
There is no requirement for the length of a single film.
There is a requirement for the minimum length to be radiographic in case of spot RT (read UW-52).
Each one welder's job has to be RTed.
One spot for each 15 meters of weld has to be RTed.
The min length of the spot is 150 mm

Στις Πέμ, 19 Μαρ 2020 στις 1:10 μ.μ., ο/η 'anand gupta' via Materials & Welding <materials-welding@googlegroups.com> έγραψε:
Dear all

Please confirm the width of RT film as per ASME Sec VIII. 

Regards 

A p gupta 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/264284656.692462.1584613280413%40mail.yahoo.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40BTWeoCScqVXmGAyGR3U-GuC7PJs85%3Dv5N21dZVd6X3PA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...