IS2062 E250 is assigned to P-No1, Grp No 1 (see Non Mandatory App. D of the Section IX)
However, there is no P-No assigned to E350, so  you need a new PQR

Στις Πέμ, 19 Μαρ 2020 στις 2:53 μ.μ., ο/η Somnath Ashtakar <s.ashtakar@gmail.com> έγραψε:
Hi,

We have qualified WPS as per ASME SEC IX for material IS 2062 E250 material , now we want to weld material IS2062 E350 material, Can we use the same WPS ?

as IS 2062 E250 - Tensile strength - 410 MPA & 
IS2062 E350 - Tensile strength - 490 MPA

Please suggest your views.. Urgent.

--
Thanks and Regards,
Somnath Ashtakar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAA484EZny6OtkXX518AU1hqCmO9J5gGU69nvMAX%3D-7v8PLfOmA%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40AekBiMN630gVn7MMEHsr0NYBMtDsATnhdGMLkwB67%3DZQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...