For projects in middle east it is almost mandatory that a TPI is used although it is not a code requirement. In other countries u may follow what is prevailing in those countries.

Thanks & Rgds.
Prakash Gotimukul
Authorised Inspection Supervisor
AIA LLC TX USA
MOB +97155 7114671
           +919730039755

On Thu, Mar 26, 2020, 13:56 Vinay Thattey <vinay.thattey@gmail.com> wrote:
Nice explanation , Mr Ramesh

On Tue, 24 Mar 2020 at 08:37, Ramesh <rameshkannandevaraj@gmail.com> wrote:
Each organisation can certify WPS/PQR. refer ASME Sec-IX- QW 201,  TPI review/witness is NOT mandatory,

TPI review / witness is Not code requirements, this is to satisfy customers that they have qualified WPS/PQR  upfront with third party check than vendors own personal. 

Also note, code allows SWPS - Prequalified WPS, means u can understand that does not require TPI involvement ! 


Thanks and Regards

Rameshkannan Devaraj

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"



On Mon, Mar 23, 2020 at 3:06 PM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
No. TPI can witness PQR and can review WPS. TPI can't Certify PQR and can't Approve WPS. In ISO as examining body, they can certify WPQR not WPS. 

On Sun, 22 Mar 2020 12:38 pm Venkat Ramana, <venkatgps.ramana@gmail.com> wrote:
The contracted prepared and qualified as per AWSD1. 1 edition 2015 and ASME Sec IX edition 2015. Is there any requirement to do the sign on WPS copies??

Please clarify.... 

Venkat

On Sat, Mar 21, 2020, 12:29 PM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
Not necessarily. But as per 2019, competent welding personal should be available to review welding related documents within company. 

On Sat, 21 Mar 2020 9:34 am Venkat Ramana, <venkatgps.ramana@gmail.com> wrote:
Dear Experts,

My query is that, is there any mandatory by TPI approval (Seal and Sign) on every WPS ?? even though they have already sign into the supporting PQR'S....

KINDLY CLARIFY WITH RELEVANT CODES AND STANDARDS.


Thanks & Regards

Venkat
+91 9676061257

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHAXWsPJvRAQu5%3DeNN0L8qFX_-SjVMCK-YAkoQ2AjshHsBmPdw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePi1hUtNnLbEdw6tT-vPZq8wPbTgQCbvYR8xfP7fbr2eQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHAXWsOHNyJEOu7CKyA62d7_vGtwonZ6g-9tUkMzGyLsOajiRQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMhbPUbSBZj156rMD%3D6y4Qpq6a1h%2BOpCiOiJLMvxn-ApA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMaSVcFcxi4PfXwvhAgPZCZHiCHCARw%2BSXoH%3DAijFi38x28o7w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BQ29OgfihoFZkoTKtiotyfTMf3qv%2BSmEn%3D%2BUPGdUUY_E%2BcjVw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOUP4q%2Bx%2B1DKrCTeFR5hRzqPDupLNrx61QmoW7-bD%3DXP_cBStw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...