Tuesday, March 24, 2020

Re: [MW:30653] Mechanical properties for SAE 1018 grade material

Thank you very much for the information shared

On Tuesday, 24 March 2020 08:37:27 UTC+5:30, metmel wrote:

1018 is an AISI designation that specifies chemistry only although standards other than the general ASTM/SA-A29 might specify.  AISI 1018 is a carbon steel with a nominal carbon content of 0.18%.

 

For example:

 

A/SA-311  Specification for cold-drawn, stress-relieved carbon steel bars subject to mechanical property requirements

 

Varies on diameter/thickness

Thickness/diameter

in. (mm)

Tensile

ksi (MPa)

Yield

ksi (MPa)

Elongation - RA

< 7/8 (20)

70  (480)

60  (415)

18 - 40

>7/8 (20) to < 1¼ (30)

65  (450)

55  (380)

16 - 40

>1¼ (30) to < 2 (50)

60  (415)

50  (345)

15 - 35

>2  (50) to < 3 (75)

55 (380)

45 (310)

15 - 35

 

 

 

 

 

You might also look at other specifications referenced in A/SA-29.

 

Hope this helps.  Code is fun.  "Live long and prosper" (Mr. Spock)

 

 

From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of SURESH
Sent: Monday, March 23, 2020 4:36 AM
To: Materials & Welding
Subject: [MW:30648] Mechanical properties for SAE 1018 grade material

 

Dear Expert

I am having below clarification

 

What is the mechanical properties for below said grade material, which standard to refer

1.SAE 1018

2. ASTM A29, Grade:1018

 

 

 

Regards

Suresh

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a7066f2f-0075-4d37-9c9c-f28526554fcc%40googlegroups.com.

DISCLAIMER This e-mail and any attachments thereto may contain information which is confidential and/or protected by intellectual property rights and are intended for the sole use of the recipient(s)named above. Any use of the information contained herein (including, but not limited to, total or partial reproduction, communication or distribution in any form) by persons other than the designated recipient(s) is prohibited. If you have received this e-mail in error, please notify the sender either by telephone or by e-mail and delete the material from any computer.
General Data Protection Regulation (GDPR)
We respect and protect your privacy to provide you with our services. Please read https://www.hamon.com/customer-data-protection-notice (Customer) and https://www.hamon.com/seller-data-protection-notice (Supplier) how we process your personal data.

Thank you for your cooperation.
______________________________________________________________________

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/dacd5b25-14f3-4e4d-9b58-e1ce194bc60a%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...