The contracted prepared and qualified as per AWSD1. 1 edition 2015 and ASME Sec IX edition 2015. Is there any requirement to do the sign on WPS copies??

Please clarify.... 

Venkat

On Sat, Mar 21, 2020, 12:29 PM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
Not necessarily. But as per 2019, competent welding personal should be available to review welding related documents within company. 

On Sat, 21 Mar 2020 9:34 am Venkat Ramana, <venkatgps.ramana@gmail.com> wrote:
Dear Experts,

My query is that, is there any mandatory by TPI approval (Seal and Sign) on every WPS ?? even though they have already sign into the supporting PQR'S....

KINDLY CLARIFY WITH RELEVANT CODES AND STANDARDS.


Thanks & Regards

Venkat
+91 9676061257

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHAXWsPJvRAQu5%3DeNN0L8qFX_-SjVMCK-YAkoQ2AjshHsBmPdw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePi1hUtNnLbEdw6tT-vPZq8wPbTgQCbvYR8xfP7fbr2eQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHAXWsOHNyJEOu7CKyA62d7_vGtwonZ6g-9tUkMzGyLsOajiRQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...