Thursday, March 19, 2020

Re: [MW:30637] IS2062E250 WPS FOR IS2062E350

IS 2062 E250 - Tensile strength - 410 MPA & 
IS2062 E350 - Tensile strength - 490 MPA

The criterion is not only the Tensile strength, but also the metallurgical similarity, that is the reason why the P Numbers exist, but These materials do not have P Numbers assigned, see Table QW-422.
Saludos!

El jue., 19 mar. 2020 a las 8:25, Charles Jacob (<charlesvj@gmail.com>) escribió:
Dear, 

If you have qualified a base metal in a particular tensile strength, with a PNo. Then a metal with the same P No but higher tensile is not possible to weld. Your WPS cannot guarantee that weld is safe at higher tensile strengths. 


Hope this helps

Regards, 

Charles V Jacob 

On Thu, Mar 19, 2020, 4:53 PM Somnath Ashtakar <s.ashtakar@gmail.com> wrote:
Hi,

We have qualified WPS as per ASME SEC IX for material IS 2062 E250 material , now we want to weld material IS2062 E350 material, Can we use the same WPS ?

as IS 2062 E250 - Tensile strength - 410 MPA & 
IS2062 E350 - Tensile strength - 490 MPA

Please suggest your views.. Urgent.

--
Thanks and Regards,
Somnath Ashtakar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAA484EZny6OtkXX518AU1hqCmO9J5gGU69nvMAX%3D-7v8PLfOmA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKpzM4D2yE8-vLFDTVXZozX4vACjosp9uR2cJKCxdqqT0xx-3Q%40mail.gmail.com.


--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SSI-TPI

Móvil +52 1 812 352 4606

Skype: jjjimeneza





--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5ZurLABZ9UPKj6-z7trkvEi5rLLuZ5Z9wCmmfWX9H_E2m2tw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...