I do not think that a factory pipe, which must have the manufacturer's name, heat, specification, diameter and schedule, have to bring a Partial Data Report, I have never seen such a thing, but ask your assigned Authorized Inspector .

El lun., 16 mar. 2020 a las 3:39, chiluka venkatramulu (<ramuluchiluka@gmail.com>) escribió:
Dear All,
Pl clarify the below requirement.
If welded pipe required in U-stamp job, is the pipe manufacturer should have U-stamp certification?. Such material must be furnished with a Code Partial
Data Report for Welded Construction (Form U-2 or U-2A)?

Thanks & Regards,
Venkatramulu CH

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF98%2BdHm2ve87wD_F_KN6usSXo%2Bfe4OLA-Ozqig6Hdo%3DNYBbMw%40mail.gmail.com.


--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SSI-TPI

Móvil +52 1 812 352 4606

Skype: jjjimeneza





--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5Zur%2BkirJQqxvBETEvy-9w2czdNBbTeoSZrtnksdXxB_%3DiCQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...