Ref B 31.3-2018,  341.4.2. Examination- Category D Fluid

On Mon, 9 Mar 2020 8:49 pm Prasanta Kumar Pal, <palpk07@gmail.com> wrote:
RT does not depend upon only category of fluid. See the other criteria.

On Mon, 9 Mar 2020 at 1:45 PM, sid <saeedsid8612@gmail.com> wrote:
Dear all,

Need answer of this below question please help out with correct answer.

*Extent of radiography for catagory D fluid? 


Regards
Sid

On Friday, 28 March 2014 15:27:30 UTC+3, ELAMARAN RAJAN wrote:
Dear Experts

What is the Radiography requirement for category D fluids with
reference to B31.3

Regards
--
maran

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/eaff11fd-d447-4129-8feb-a71fc295999c%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANm_%2BDh045%2BW6%3DcSYgjUbTd-MSCv7%2BiymbnmtBitmTF2EeQ_ig%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNoY58y-N5zmOpj7e8QGS5rYfzh7tN78nyzdH4p53-2PA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...