Monday, March 9, 2020

Re: [MW:30614] Re: RT requirement for cat D fluids

Hi ,

Radiography is not required for category "D" fluid as per ASME B 31.3.

Best Regards
Atul Khatri

On Mon, Mar 9, 2020 at 1:45 PM sid <saeedsid8612@gmail.com> wrote:
Dear all,

Need answer of this below question please help out with correct answer.

*Extent of radiography for catagory D fluid? 


Regards
Sid

On Friday, 28 March 2014 15:27:30 UTC+3, ELAMARAN RAJAN wrote:
Dear Experts

What is the Radiography requirement for category D fluids with
reference to B31.3

Regards
--
maran

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/eaff11fd-d447-4129-8feb-a71fc295999c%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACKOSeC0skWRS2fnhYSniQ2bXKBjvDtUGDZN9GrUQ-zyzK2Rkg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...