Re: [MW:30607] Opening of Nozzle in Weld in Dished End.

You have not mentioned joint effect. If the construction is with full radiography, you can go ahead.
N. S. Pandit

On Fri, 6 Mar 2020, 10:44 Kannayeram Gnanapandithan, <kgpandithan@gmail.com> wrote:
Dears
         Construction Code-ASME Sec 8, Div-1.   Nozzle hole is fouling in the  Welding of Dished End Petal Construction. Is it permissible?. Throw your valuable inputs. 
 
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePwMfsfsPEWEwe8beOO8NQVY-8EPrkxMc%3DF_jFFKnV6hA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB7ASHf3kOfaPLet9321TX_grE9Qbzx95EoO%2B9tLmXsYfRMRsQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...