Re: [MW:30607] Impact test for PQR

What is the version(year)  of code.

Thanks & Regards

J.Gerald Jayakumar




On Friday, March 6, 2020, 12:15:24 PM GMT+7, Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:


Ref the below attachment taken from ASME sec 8, Div1, UG 84, h, 5.  Hope that it will clear your doubts. 

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Tue, Mar 3, 2020 at 10:37 AM Chintan <chintan51@gmail.com> wrote:
Kindly advice how many set of impact test (for each process)needs to run to qualify PQR with below details
What is code ref for pqr impact test

Base metal  thick 50 mm
Process GTAW (5mm) + FCAW (20 mm) + SAW (25 mm)
Governing code asme sec 8 div 1 & asme sec 9
MDMT minus 29 deg cel

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/be15deb6-c237-4b43-9194-cdb198cb41a0%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNnwg-ycaayn_fX7xRd44LgSOB%2BcemrGQr2ETSdQQtjKg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...