Tuesday, March 3, 2020

Re: [MW:30585] Impact test for PQR

Sorry.

Regarding the last edition of ASME VIII, there is specific mention to multiple processes. 

Best regards

Em ter., 3 de mar. de 2020 às 10:15, Fernando L Neto <fernando.lescovar@gmail.com> escreveu:
Hello, colleagues. 

This is also my doubt. 

UG-84 does not require impact sets for each process. quantity of sets is defined only based on base metal thickness. Am I correct? 

Are additional impact sets for each process supplementary requirement in addition to ASME requirements? 

Best regards, 

Em ter., 3 de mar. de 2020 às 02:07, Chintan <chintan51@gmail.com> escreveu:
Kindly advice how many set of impact test (for each process)needs to run to qualify PQR with below details
What is code ref for pqr impact test

Base metal  thick 50 mm
Process GTAW (5mm) + FCAW (20 mm) + SAW (25 mm)
Governing code asme sec 8 div 1 & asme sec 9
MDMT minus 29 deg cel

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/be15deb6-c237-4b43-9194-cdb198cb41a0%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANv%2BETYhmFCXUfnj0Vwj9mPxFt0ETAx6-8kphBqfXcT%3DsFeGUg%40mail.gmail.com.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...