Re: [MW:30330] Re: Filler material Selection

While welding CS with 316, ( chemistry 19Cr+12Ni), there is loss in Cr and Ni more 316 when compare with 309( 24Cr+13). For maintaining austenetic structure in ASS( as per code B31.1, which is attached) minimum requirement of Ni is 8, which may not be achievable with 316. So, it is better to use 309 instead of 316


THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Fri, Dec 27, 2019 at 11:45 AM Jason <haiyuqingkong@gmail.com> wrote:
ASTM A106 Gr.B  is Carbon steel,E316L electrodes are used for stainless steel

在 2019年12月23日星期一 UTC+3上午8:25:39,Navanith写道:
Dear Experts,

Require guidance on filler material selection as per ASME BPVC.
For example:I received this query from a client
Base metal is ASTM A106 Gr.B and they want to weld using E316L electrodes.
Is it possible to use E316L electrodes to weld directly?

Regards,
Navanith

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/fc4d2cad-60ca-4f48-819d-44f5d0d9cda7%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMnxqu7RrnK02J7Wcmmu2%2BjkzguUTp3m5MqjeZSUubiDw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...