Skip to main content

Re: [MW:30324] PSV set pressure during hydrotest of piping

Hi, 

Expert, please see the below your answer...as per Saudi Aramco Standard, SAES-A-004 Para 5.7.

Protection from Overpressure
All systems (piping and equipment) while being pressure tested shall be protected from being over pressured by the following:

Pressure test relief valve(s) of adequate capacity set to relieve at 5% above the test pressure shall be installed unless the test pressure is less than 85% SMYS at which time it can be set at 10% above the test pressure. Sizing of these relief valves used for testing shall follow the requirements of API RP 520, Part 1. The relief valve(s) shall be tested, dated, and tagged within two weeks prior to the pressure test for new construction projects, and within three months for maintenance operations.
The pressure test relief valve shall be accompanied with a calibration certificate that includes the cold differential test pressure (CDTP), test date and the spring range. The CDTP shall be within the spring range.
Pressure testing relief valves shall be car sealed at the pressure adjusting screw and verified prior to test.

Thank you for your consideration. I look forward to hearing from you. Your Immediate Response will be Highly Appreciated.

Best Regards

Shrichand Ghanshyam Bathv 

Mobile Number : +91 8551911459

Email Id : shrichand.bathv@gmail.com 

Skype Id : shrichand.bathv 

-------------------------------------------------------------

"Success doesn't come to you... you go to it. "

"Helping hands are better than praying lips. "

--------------------------------------------------------------

P please consider the environment before printing this mail note.

*******************************************************************






On Thu, Dec 26, 2019 at 2:19 PM Balajirajan Palanisamy <pbrerode@gmail.com> wrote:
Dear Mr. Manoj,
   During the Hydro test the set pressure of PSV that you had fixed in the manifold will be as 1.1 times of the line test pressure i.e 10% higher than the line test pressure. 

Regards,
P.Balajirajan.

On Tue, Dec 24, 2019 at 11:59 AM Eyup Tan <eyuptan@gmail.com> wrote:
You should blank PSV during the hydro test or remove PSV from line/equipment. 
Because PSV set pressure is adjusted to %10 above of MAWP. But hydrostatic Test Pressure is 1,5 times of MAWP.
You can't make hydrostatic test 1,5 times of MAWP because PSV will open when pressure comes to 1.1 times of MAWP. 
That is why you need to blank or remove PSV during the hydro test

Saygılarımla, / Best Regards,

Eyup Tan

Mobile: +90 535 334 4912


On Tue, Dec 24, 2019 at 11:14 AM ViNo Varughese <vinopvarghese@gmail.com> wrote:
Dear Manoj,

Please check through API RP 520 and you should find the set pressure requirement for PRVs. Typically it is set based on the MAWP or  design pressure. However you also need to consider the static head between the protected equipment and the relied valve while deriving the set pressure.

Hope this helps.


Thanks and Regards
Vino



On Tue, Dec 24, 2019, 08:23 Manoj John <manojacgnr@gmail.com> wrote:
Dear Experts,

As per B31.3 what is the PSV set pressure during hydrotest.
Please give expert opinion as there is no clause found in B31.3 for hydrotest PSV set pressure, PSV set pressure for pneumatic only prescribed.

Thanks in advance,
Manoj

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACgUO5nJ9-S1uDxZVTxg%2BYRcsUy8F64M-QRiugW%2BKbmYx6s8Lw%40mail.gmail.co

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM7oz7DLt%2Bn_Rq50i7a7iLO7S2M%3D1V9N_128874eoR4%3DdzB8RQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPfEVaMG7SqoLwdHG23YCZDgUs%3D%2B8PSb17O7izvW96%2B%3DMX%3D6_A%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEXdmd_HgLY0pxzUSshMY1VJszviPB1wgy%2BvHmqUL3VD8Gpmxw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKrxSc9FkYqEnqrHCULHTo69fs-9m-WtRscNpbH8hgyxDhtOmg%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...